Klasifikasi AWS: AWS 5.9
KATERANGAN:
Kawat las stainless steel mibanda efisiensi cladding anu luhur, kinerja téknis las anu saé dina las sadaya posisi. Kawat ieu seueur dianggo dina industri: struktur wangunan, kendaraan, rékayasa sasak, mesin pertambangan, jalur karéta api, pipa minyak, peralatan bantalan tekanan gas, peralatan listrik, jsb.
NOMOR & UKURAN MODEL:
1. Layanan OEM suplai pabrik.
2. Modél: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi jsb.
3. Ukuran kawat MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.
4. Ukuran kawat TIG: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm.
BUBUKA:
Kami nyayogikeun rupa-rupa kawat las stainless steel, kalebet kawat las padet Mig, kawat las batang Tig sareng kawat las busur terendam, sadayana kualitas luhur sareng dijual di sakumna dunya.
Iwal ti 308 sareng 309, kami ogé nawiskeun 304, 321, 347, 316L, 310, 2209, sareng 201. Salian ti spésifikasi khusus sapertos 318L, 904L, 2594, NiCrMo-3, Ni1.
PAKET:
Kawat las Mig dibungkus (bungkus spool sareng drum)
Diaméter: 0,8 - 2,0mm
Pakét: 1 kg/gulungan, 5 kg/gulungan, 15 kg/gulungan, 20 kg/gulungan, 100 kg/drum, 200 kg/drum
Kawat las batang tig dibungkus (tabung plastik)
Diaméter: 1.0 - 5.0mm
Pakét: 5 kg/pak
Kawat las busur anu tilelep
Diaméter: 2,5 - 5,0mm
Pakét: 20kg/pak, 25 kg/pak
Bungkusan nétral sareng OEM wilujeng sumping!
KOMPOSISI KIMIA KAWAT LAS STAINLESS STEEL:
| Modél No. | C | Si | Mn | P | S | Cr | Ni | Mo | Cu |
| 304 | 0.08 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-11.00 | 0.18 | 0.003 |
| 304L | 0.03 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-12.00 | ||
| ER307 | 0.04-0.14 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 8.00-10.70 | 0.5-1.5 | 0.75 |
| ER308 | 0.08 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 9.00-11.00 | 0.75 | 0.75 |
| ER308L | 0.03 | 0.30-0.65 | 1.50-2.30 | 0.03 | 0.02 | 19.5-21.5 | 9.00-11.00 | 0.75 | 0.75 |
| ER308LSi | 0.03 | 0.65-1.00 | 1.60-2.40 | 0.03 | 0.02 | 19.5-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER309 | 0.12 | 0.30-0.65 | 1.00-2.50 | 0.03 | 0.03 | 24.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER316 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 18.00-12.00 | 11.0-14.0 | 2.0-3.0 | 0.75 |
| ER316L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER316LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER310 | 0.08-0.15 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 25.0-28.0 | 20.0-22.5 | 0.75 | 0.75 |
| ER347 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 19.0-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER317 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.01 | 18.5-20.5 | 13.0-15.0 | 3.0-4.0 | 0.75 |
| ER321 | 0.08 | 0.3-0.65 | 1.5-2.5 | 0.03 | 0.01 | 18.5-20.5 | 9.0-10.5 | 0.75 | 0.75 |
| Modél No. | Kakuatan tarik Rm (Mpa) | Kakuatan hasil Rel atanapi Rp0.2 (Mpa) | Pemanjangan (%) | Modél No. | Kakuatan tarik Rm (Mpa) | Kakuatan hasil Rel atanapi Rp0.2 (Mpa) | Pemanjangan (%) |
| 304 | 550 | -- | 25 | ER309LSi | 510 | 320 | 25 |
| 304L | 510 | -- | 25 | ER316 | 510 | 320 | 25 |
| ER307 | 590 | 350 | 25 | ER316L | 510 | 320 | 25 |
| ER308 | 550 | 350 | 25 | ER316LSi | 510 | 320 | 20 |
| ER308L | 510 | 320 | 25 | ER310 | 550 | 350 | 25 |
| ER308LSi | 510 | 320 | 25 | ER347 | 550 | 350 | 25 |
| ER309 | 550 | 350 | 25 | ER317 | 550 | 350 | 25 |
| ER309L | 510 | 320 | 25 | ER321 | 550 | 350 | 25 |
| Komposisi kawat las stainless steel TIG sareng MIG | ||||||||||
| YB5092-2005 | AWS | Komposisi Kimia % | ||||||||
| C | Si | Mn | P | S | Cr | Ni | Mo | |||
| H08Cr20Ni9Mn7Si | ER307Si | 0.075 | 0.78 | 6.7 | 0.022 | 0.01 | 19.8 | 8.8 | ||
| H06Cr21Ni10 | ER308 | 0.045 | 0.45 | 1.9 | 0.02 | 0.009 | 20.8 | 9.8 | ||
| H0OCr21Ni10 | ER308L | 0.02 | 0.32 | 1.9 | 0.011 | 0.006 | 20 | 10.2 | ||
| H06Cr21Ni10Si | ER308Si | 0.045 | 0.85 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | ||
| H06Cr24Ni13 | ER309 | 0.06 | 0.45 | 1.9 | 0.019 | 0.009 | 24.3 | 13.2 | ||
| H06Cr24Ni13Si | ER309Si | 0.06 | 0.79 | 1.95 | 0.019 | 0.009 | 24.7 | 13.2 | ||
| H03Cr24Ni13 | ER309L | 0.02 | 0.42 | 1.8 | 0.02 | 0.01 | 24.8 | 13.2 | ||
| H03Cr24Ni13Si | ER309LSi | 0.018 | 0.8 | 1.7 | 0.02 | 0.01 | 23.5 | 13.5 | ||
| H21Cr16Ni35 | ER330 | 0.2 | 0.38 | 1.5 | 0.022 | 0.01 | 16.5 | 34.5 | ||
| H06Cr19Ni12Mo2 | ER316 | 0.04 | 0.4 | 1.9 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H06Cr19Ni12Mo2Si | ER316Si | 0.05 | 0.7 | 1.92 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H03Cr19Ni12Mo2 | ER316L | 0.019 | 0.38 | 1.8 | 0.018 | 0.01 | 19.8 | 12.2 | 2.5 | |
| H03Cr19Ni12Mo2Si | ER316LSi | 0.06 | 0.85 | 1.7 | 0.022 | 0.01 | 18.8 | 12.6 | 2.4 | |
| H03Cr17Ni14Mo3 | ER317L | 0.02 | 0.38 | 1.8 | 0.02 | 0.01 | 18.8 | 13.8 | 3.6 | |
| H08Cr19Ni12Mo2Nb | ER318 | 0.06 | 0.42 | 1.5 | 0.022 | 0.01 | 18.5 | 11.8 | 2.3 | |
| H07Cr20Ni34Mo2Cu3Nb | ER320 | 0.06 | 0.4 | 1 | 0.022 | 0.01 | 19.8 | 33.3 | 2.8 | Nb0.7 |
| H02Cr20Ni34Mo2Cu3Nb | ER320L | 0.018 | 0.33 | 1.5 | 0.013 | 0.01 | 19.8 | 33.6 | 2.5 | Nb0.35 |
| H08Cr20Ni10Ti | ER321 | 0.06 | 0.45 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | Ti9xC-1.0 | |
| H08Cr21 Ni10Nb | ER347 | 0.055 | 0.48 | 1.8 | 0.021 | 0.008 | 20.8 | 9.8 | Nb1xC-1.0 | |
| H12Cr26Ni21 | ER310 | 0.09 | 0.5 | 1.66 | 0.02 | 0.01 | 25.5 | 20.5 | ||
| H02Cr20Ni25Mo4Cu | ER385 | 0.02 | 0.3 | 1.5 | 0.018 | 0.01 | 20.2 | 24.8 | 4.8 | Cu 1.80 |
| H03Cr22Ni9Mo3N | ER2209 | 0.022 | 0.5 | 0.9 | 0.02 | 0.01 | 22.5 | 8.8 | 3.3 | N0.08-0.20 |
| H04Cr25Ni5Mo3Cu2N | ER2553 | 0.027 | 0.5 | 1 | 0.025 | 0.015 | 24.8 | 5.5 | 3.2 | N0.1-0.25 |
| H1 5Cr29Ni9 | ER312 | 0.09 | 0.38 | 1.5 | 0.022 | 0.01 | 29.5 | 8.5 | ||
| H03Cr24Ni13MoL | ER309L Mo | 0.023 | 0.45 | 1.5 | 0.022 | 0.01 | 23.8 | 13.2 | 2.2 | |
| H05Cr17Ni4Cu4Nb | ER630 | 0.04 | 0.39 | 0.5 | 0.022 | 0.01 | 16.5 | 4.8 | Cu;3 Nb;0.28 | |
| H08Cr26Ni5Mo2 | ER453s | 0.06 | 0.3 | 0.4 | 0.022 | 0.01 | 25.8 | 4.8 | 2.1 | |
| H08Cr21Ni10Mn6 | 0.06 | 0.35 | 5.5 | 0.022 | 0.01 | 20.8 | 9.8 | |||
| H05Cr22Ni11Mn6Mo3VN | ER209 | 0.04 | 0.4 | 4.5 | 0.022 | 0.01 | 21.5 | 10.8 | 2.2 | N;0.20 V;0.18 |
Wenzhou Tianyu Electronic Co., Ltd. diadegkeun dina taun 2000. Kami parantos kalibet dina manufaktur éléktroda las, batang las, sareng bahan las anu tiasa dianggo salami langkung ti 20 taun.
Produk utama kami kalebet éléktroda las stainless steel, éléktroda las baja karbon, éléktroda las paduan rendah, éléktroda las permukaan, éléktroda las paduan nikel & kobalt, kawat las baja hampang & paduan rendah, kawat las stainless steel, kawat inti fluks anu dilindung gas, kawat las aluminium, kawat las busur terendam, kawat, kawat las paduan nikel & kobalt, kawat las kuningan, kawat las TIG & MIG, éléktroda tungsten, éléktroda gouging karbon, sareng asesoris & barang konsumsi las anu sanésna.
Wenzhou Tianyu Electronic Co., Ltd. diadegkeun dina taun 2000. Kami parantos kalibet dina manufaktur éléktroda las, batang las, sareng bahan las anu tiasa dianggo salami langkung ti 20 taun.
Produk utama kami kalebet éléktroda las stainless steel, éléktroda las baja karbon, éléktroda las paduan rendah, éléktroda las permukaan, éléktroda las paduan nikel & kobalt, kawat las baja hampang & paduan rendah, kawat las stainless steel, kawat inti fluks anu dilindung gas, kawat las aluminium, kawat las busur terendam, kawat, kawat las paduan nikel & kobalt, kawat las kuningan, kawat las TIG & MIG, éléktroda tungsten, éléktroda gouging karbon, sareng asesoris & barang konsumsi las anu sanésna.