ENiFe-CI Nikel Alloy Las Kawat, FN 55 Nikel Tig Kawat Ferro-nikel Padet Kawat

Katerangan pondok:

Kawat padet ferro-nikel dipaké pikeun las beusi tuang sareng beusi ductile.


Rincian produk

Tag produk

Nikel AlloyKawat las Kawat TigENiFe-CI

Standar
EN ISO 1071 – SC NiFe-1
AWS A5.15 - E NiFe-CI

 

Fitur sarta Aplikasi

Ferro-nikelkawat padet dipaké pikeun las beusi tuang jeung beusi pangleuleusna.

Cocog jeung sendi dissimilar antara beusi tuang, baja hampang, alloy lemah sareng stainless steels.

Disarankeun pikeun las walirang tinggi, phosphorous atawa lubricant-kacemar castings.

Ilaharna dipaké pikeun sauntuyan perbaikan sarta aplikasi fabrikasi, kaasup rebuilding shafts, roda, sendi kritis antara baja jeung beusi tuang jsb.

Bahan Dasar has

Beusi tuang abu, gampang ditempa, nodular*
* Illustrative, teu daptar lengkep

 

Komposisi Kimia%

C%

Mn%

Si%

P%

S%

   

max

max

max

max

max

   

2.00

0.80

0.20

0.03

0.03

   

   

Fe%

Ni%

Cu%

Al%

   

rem.

54.00

max

max

   

56.00

2.50

1.00

   

 

Sipat mékanis
Kakuatan regangan 400 – 579 MPa  
Kakuatan ngahasilkeun -  
Elongation -  
Kakuatan Dampak -  

Sipat mékanis kira-kira sareng tiasa rupa-rupa dumasar kana panas, gas pelindung, parameter las sareng faktor sanésna.

 

Gas pelindung

EN ISO 14175 - TIG: I1 (Argon)

 

Posisi las

EN ISO 6947 - PA, PB, PC, PD, PE, PF

 

Data bungkusan

Diameter

Panjangna

Beurat

1,60 mm

2,40 mm

3,20 mm

1000 mm

1000 mm

1000 mm

5 Kg

5 Kg

5 Kg

Tanggung jawab: Samentawis sadaya usaha anu wajar parantos dilakukeun pikeun mastikeun katepatan inpormasi anu dikandung, inpormasi ieu tiasa robih tanpa aya bewara sareng ngan ukur tiasa dianggap cocog pikeun pedoman umum.

 


  • saméméhna:
  • Teras: